Tube for Perforating Gun
Tube for Perforating Gun is the main raw material for manufacturing various high-performance oil and gas well perforating guns. The tube for Perforating Gun not only withstands the high-speed impact of perforating bullets during perforating operations, but also bears the reverse impact of perforating bullet fragments on the pipe.
In this way, not only the impact toughness of the perforating barrel is very high, but also the yield strength is also very high to withstand high impact loads.
Uses
For manufacture of perforating gun body
Standard
YB/T 4371-2014 Seamless steel tubes for perforating guns for oil and gas wells
Product Size
Outside Diameter and wall thickness of Tube for Perforating Gun
Outside Diameter, mm |
Wall Thickness, mm |
73.00 |
5.51, 7.82, 9.19 |
82.50 |
9.00 |
83.00 |
9.00 |
88.90 |
6.45, 7.10, 8.00, 8.80, 9.19, 10.00, 12.00 |
95.00 |
8.00, 10.00 |
96.00 |
10.00 |
101.60 |
7.00, 9.00, 9.50, 10.00, 11.00 |
108.00 |
8.00 |
114.30 |
8.50, 9.50, 10.00, 11.10, 12.50, 13.00 |
127.00 |
9.50, 11.00, 12.50 |
Length of Tube for Perforating Gun: 8-12m
Chemical Composition(%)
Chemical Composition of Tube for Perforating Gun
Grade |
C |
Si |
Mn |
P |
S |
Cr |
Mo |
V |
32CrMo4 |
0.29-0.36 |
0.07-0.37 |
0.50-0.80 |
<0.015 |
<0.010 |
0.90-1.20 |
0.20-0.30 |
|
25Mn2MoV |
0.21-0.29 |
0.15-0.50 |
1.30-1.90 |
<0.015 |
<0.010 |
|
0.10-0.30 |
0.05-0.20 |
Mechanical Properties
Mechanical Properties of Tube for Perforating Gun
Grade |
Elongation
% |
Yield Strength
MPa |
Tensile Strength
MPa |
Transverse
Impact, J |
Longitudinal
Impact, J |
Hardness
HRC |
GL-PG110 |
≥17 |
758-965 |
≥862 |
42 |
84 |
26-33 |
GL-PG130 |
≥14 |
896-1103 |
≥930 |
42 |
84 |
>30 |
GL-PG140 |
≥11 |
965-1172 |
≥1000 |
42 |
84 |
>33 |
GL-PG155 |
≥10 |
1068-1275 |
≥1137 |
42 |
84 |
>33 |